Precautions for the use and maintenance of molten iron ladle
1.The molten iron ladleis lined with fire-resistant mud, and its thickness is: 0.5 t~3 t side wall, 60 mm bottom, 80 mm,
5 t side wall, 80 mm bottom, 100 mm, 10 t side wall, 100 mm bottom, 120 mm
m, 10 t side wall,>150 mm bottom,>180 mm
2. Check the hand wheel, and it should be free from jamming
3. In the two trunnion rolling bearings, Add molybdenum disulfide lubricating grease once a week
4. Check whether the locking chuck of the hand wheel is safe and reliable
5. Check whether there is oil shortage in the reducer box. Check once a week
6. When the worm gear pair clearance is found to be increased after using for a long time, which hinders the safe casting, Worm gear should be replaced
molten iron ladle, widely used in the casting industry; After receiving molten iron in front of the furnace, it is transported to the mold by crane for pouring
Features of molten iron ladle:
1. The molten iron ladle adopts double worm gear pair transmission, which is flexible and free, and has good bidirectional reversibility
2. The rotating center of the ladle is reasonably selected. It is easy to operate and can be redone after pouring
3. The suspender of the molten iron ladle is forged, which is more reliable and safe than the steel plate weldment
4. The ladle body steel plate is thick, and the ladle bottom adopts a triple safety structure of taper, bottom hoop and welding, which extends the service life and ensures the safety of the operator
5. The main body of the ladle and the suspender, the reduction gearbox and the handwheel are all equipped with chain clamping plates which can be locked at any time
6. The two trunnions and suspenders are equipped with self-aligning bearings in the direction, with good consistency p>